Abstract: 

In this study, a novel disruptive technology has been proposed to address two major environmental concerns: mitigating CO2 emissions from hard-to-abate industries and preventing the unplanned disposal of metal-rich industrial wastes, including e-waste and steel-industry byproducts. The proposed process is based on carbon capture and utilization (CCU), in which captured CO2 is utilized to facilitate the leaching of metal-rich wastes and the recovery of valuable metals such as Cu, Zn, Li, Co, and Ni. CO2 is absorbed into an aqueous ammonia solution in a packed-bed column equipped with a solvent recirculation system to achieve the desired CO2/NH3 molar ratio.
 

Mass transfer coefficients in packed-bed columns for gas absorption have been studied by numerous researchers. However, these studies were conducted with a continuous liquid-flow system with a fresh absorbent. The first objective focuses on investigating the overall mass transfer coefficient in a packed-bed column for a solvent recycling system (equivalent to a semi-batch process) where CO2 concentration is continuously built up in the solution. This study investigates the mass transfer behaviour of aqueous ammonia during CO2 absorption in a packed-bed absorber, under continuous CO2 loading. The overall mass transfer coefficient of CO2 absorption by aqueous ammonia was investigated based on the free ammonia concentration or CO2 loading in the solution during a recycling process in a packed-bed absorber. Experimental conditions covered a wide range of gas flow rates (76.4–367 m3m−2h −1 ), liquid flow rates (4.8–20.8 m3m−2h −1 ), and ammonia concentrations (2–10 wt.%). The volumetric overall mass transfer coefficient (KGav ) was evaluated, revealing that higher liquid flow rates and ammonia concentrations significantly enhance KGav. Gas flow rate was also found to play a significant role. Initially, KGav increased with increasing gas flow rate; however, at higher gas flow rates, KGav decreased. The KGav values for CO2-loaded ammonium solutions were compared with those obtained using fresh ammonia solutions. Increasing CO2 loading reduced KGav because of the decline in free NH3 concentration. Furthermore, KGav was found to exhibit an approximately linear dependence on the free ammonia concentration. This near-linear dependence, stronger than the square root dependence on free ammonia concentration (WNH3 0.5) predicted by pseudo-first-order theory, was attributed to operation in the intermediate reaction regime at high ammonia concentrations and CO2 partial pressures. An empirical correlation has been proposed between the volumetric overall mass transfer coefficient and the investigated experimental parameters for the present system as follows: KGav ∝ WNH3 L 0.3G 0.33 where L and G correspond to liquid flow rate and gas flow rate, respectively, m3 . m−2
. h −1.

Secondly, the resulting solution, containing free ammonia and ammonium salts (carbamate, carbonate, and bicarbonate, depending on the CO2/NH3 molar ratio) is a good scavenger for metal extraction. Zinc ash, a zinc-rich byproduct of the steel and galvanizing industries, was used as feedstock for zinc recovery. The effects of various process parameters, including the
CO2/NH3 molar ratio (0-0.6 mol/mol with 4-20 wt.% of total NH3 concentration), temperature (5-80 °C), stirring speed (200-1000 rpm), H2O2/Zn molar ratio (0-1.8 mol/mol), and liquid-to -solid ratio (5-20 mL/g) were investigated to optimize the leaching conditions. Kinetic study using the shrinking core model indicated that zinc leaching in ammoniacal solution was best
described by the product-layer diffusion-controlled model, with an apparent activation energy of 16.53 kJ/mol. Zinc was recovered from the leached solution (leachate) as basic zinc carbonate (a stable form of the zinc salt) by heating. The ammonia vapor released during heating was captured in a packed-bed scrubber, and the recovered ammonia could be reused in
the CO2 absorption process. Overall, a sustainable closed-loop CCU process was developed, achieving a zinc leaching efficiency of over 90%, ammonia recovery of approximately 99% during the solvent recovery step, and utilization of approximately 30% of the CO2 captured in the solution during zinc extraction from the waste.

.